Stainless Steel Stick Electrodes: Aws E309-16 Aws E309Mo-16 Aws E309Mol-16

Download as pdf or txt
Download as pdf or txt
You are on page 1of 10

Stainless Steel

Stick Electrodes

308/308H Sterling AP 309 H Sterling AP 309Mo


308/308H DC Lime AWS E309-16 309MoL AC-DC
The moisture resistant, all-position 309 (H)
308/308H Sterling® Sterling® AP electrode is primarily designed AWS E309Mo-16
for welding Type 309 metal but can also be AWS E309MoL-16
AWS E308-16 & E308H-16
used for 18-8 clad steels or dissimilar Addition of Molybdenum to 309 for improved
AWS E308-15 & E308H-15 tensile strength and resistance. Used for 316
materials if the alloy content is sufficently
AWS E308-17 & E308H-17 clad steels and joining Mo-containing steels
high for a sound, ductile deposit. It yields a
For applications where service conditions are to carbon steels:
uniform weld bead that is flat to slightly
not severe. Intermediate layer prior to AWS Spec A5.4, ASME SF5.4 (F-5, A-8)
convex:
deposition of hard-facing material. Use on
AWS Spec A5.4, ASME SF5.4 (F-5, A-8)
Types 301, 302, 304, 305, and 308 base Typical Deposit Analysis %
metals. Approvals and conformances: AWS
Typical Deposit Analysis % C – 0.03
Spec A5.4, ASME SFA5.4 (F-5, A-8)
C – 0.08 Mn – 1.23
Typical Deposit Analysis % Cr – 23.50 Si – 0.44
Ni – 13.00 Cr – 22.70
C – 0.06 Ni – 13.60
Mo – 0.10
Mn – 01.14 Mo – 2.40
Mn – 1.05
Si – 0.44 Fe – Bal.
P – 0.020
Cr – 19.88
S – 0.016
Ni – 9.78
Cu – 0.10 Typical Properties and Ferrite Number of
Fe – Bal.
Weld Deposit as Welded
Typical Properties and Ferrite Number of
Typical Properties and Ferrite Number of Tensile Strength . . . . . . . . . . .90,000 psi
Weld Deposit as Welded
Weld Deposit as Welded Yield Strength . . . . . . . . . . . . .70,000 psi
Tensile Strength . . . . . . . . . . .88,000 psi Elongation in 2" . . . . . . . . . . . . . . .35%
Tensile Strength . . . . . . . . . . .86,000 psi
Yield Strength . . . . . . . . . . . . .67,000 psi DeLong Ferrite Number . . . . . . . . . . . .13
Yield Strength . . . . . . . . . . . . .65,000 psi
Elongation in 2" . . . . . . . . . . . . . . .37%
Elongation in 2" . . . . . . . . . . . . . . .45%
DeLong Ferrite Number . . . . . . . . . . .6-15
DeLong Ferrite Number . . . . . . . . . . . . .7

308/308L Sterling AP 309/309L Sterling AP 310 AC-DC


308/308L DC Lime 309/309L DC Lime AWS E310-16
For welding base metal of similar
308/308L Sterling® 309/309L Sterling® composition, when the stainless base metal is
308L Smootharc Plus 309L Smootharc Plus of unknown composition, and for dissimilar
metals. Used as a transition layer for high
AWS 308/E308L-16 AWS 309/E309L-16 restrained joints of high carbon steels.
AWS 308/E308L-15 AWS 309/E309L-15 Approvals and conformances: AWS Spec A5.4,
AWS 308/E308L-17 AWS 309/E309L-17 ASME SFA5.4 (F-5, A-9)
For welding Type 308L. Properties similar to Low C modification of standard Type 309
Type 308 with low C to avert carbide analysis used for weld overlay or welding Typical Deposit Analysis %
precipitation and inhibit subsequent carbide stainless to mild or low alloy steels. C – 0.14
precipation. Approvals and conformances: Approvals and conformances: AWS Spec A5.4, Mn – 2.02
AWS Spec A5.4, ASME SF5.4 (F-5, A-8) ASME SFA5.4 (F-5, A-8) Si – 0.46
Cr – 26.12
Typical Deposit Analysis % Typical Deposit Analysis % Ni – 21.00
C – 0.03 C – 0.03 Fe – Bal.
Mn – 1.14 Mn – 1.32
Si – 0.43 Si – 0.41 Typical Properties and Ferrite Number of
Cr – 19.68 Cr – 23.00 Weld Deposit as Welded
Ni – 9.89 Ni – 13.50 Tensile Strength . . . . . . . . . . .86,000 psi
Fe – Bal. Fe – Bal. Yield Strength . . . . . . . . . . . . .63,000 psi
Elongation in 2" . . . . . . . . . . . . . . .40%
Typical Properties and Ferrite Number of Typical Properties and Ferrite Number of DeLong Ferrite Number . . . . . . . . . . . . .0
Weld Deposit as Welded Weld Deposit as Welded
Tensile Strength . . . . . . . . . . .83,000 psi Tensile Strength . . . . . . . . . . .79,000 psi
Yield Strength . . . . . . . . . . . . .64,000 psi Yield Strength . . . . . . . . . . . . .64,000 psi
Elongation in 2" . . . . . . . . . . . . . . .37% Elongation in 2" . . . . . . . . . . . . . . .41%
DeLong Ferrite Number . . . . . . . . . . . . .9 DeLong Ferrite Number . . . . . . . . . . . .13

12
Stainless Steel
Stick Electrodes

312 AC-DC 316/316L Sterling AP 330 AC-DC


AWS E312-16 316/316L DC Lime AWS E330-16
Welding Type 312 base metals. Excellent for Used to weld Type 330 base metal for heat
dissimilar metal joining due to high ferrite 316/316L Sterling® and creep resisting applications. Aprovals and
potentials. Approvals and conformances: AWS 316L Smootharc Plus conformances: AWS Spec A5.4, ASME SFA5.4
Spec A5.4, ASME SFA5.4 (F-5, 4-8) (F-5, A-9)
AWS 316/E316L-16
Typical Deposit Analysis % AWS 316/E316L-15 Typical Deposit Analysis %
C – 0.07 AWS 316/E316L-17
C – 0.20
Mn – 0.80 Welding Type 316L material. Properties
Mn – 1.84
Si – 0.40 similar to Type 316. Suited for urea
Si – 0.34
Cr – 28.50 environments. Approvals and conformances:
Cr – 15.30
Ni – 9.10 AWS Spec A5.4, ASME SFA5.4 (F-5, A-8)
Ni – 34.19
Fe – Bal. Fe – Bal.
Typical Deposit Analysis %
Typical Properties and Ferrite Number of C – 0.02 Typical Properties and Ferrite Number of
Weld Deposit as Welded Mn – 1.55 Weld Deposit as Welded
Tensile Strength . . . . . . . . . . .115,000 psi Si – 0.48
Tensile Strength . . . . . . . . . . .86,000 psi
Yield Strength . . . . . . . . . . . . .95,000 psi Cr – 18.20
Yield Strength . . . . . . . . . . . . .58,000 psi
Elongation in 2" . . . . . . . . . . . . . . .25% Ni – 13.00
Elongation in 2" . . . . . . . . . . . . . . .40%
DeLong Ferrite Number . . . . . . . . . . . .45 Mo – 2.27
DeLong Ferrite Number . . . . . . . . . . . . .0
Fe – Bal.

Typical Properties and Ferrite Number of


Weld Deposit as Welded
Tensile Strength . . . . . . . . . . .82,000 psi
Yield Strength . . . . . . . . . . . . .61,000 psi
Elongation in 2" . . . . . . . . . . . . . . .42%
DeLong Ferrite Number . . . . . . . . . . . . .2

316/316H Sterling AP 317L AC-DC 347 AC-DC


316/316H Sterling® AWS E317L-16 AWS E347-16
AWS E317L-17 AWS E347-17
AWS E316-16 & E316H-16
Increased molybdenum content results in Metal stabilized with columbium prevents
AWS E316-17 & E316H-17 higher tensile strength, better corrosion carbide precipitation. Better corrosion
For welding Type 316 steel. Applies where resistance, and improved high temperature resistance than Type 308. For welding Types
increased high temperature corrosion creep strength when compared with 316L. 347 and 321 steels. Good corrosion resistance
resistance of molybdenum-bearing steels are Approvals and conformances: AWS Spec A5.4, in steam or utility applications up to 1400°F.
necessary. Low FN version. Approvals and ASME SFA5.4 (F-5, A-8) Approvals and conformances: AWS Spec A5.4,
conformances: AWS Spec A5.4, ASME SFA5.4
ASME SFA5.4 (F-5, A-8)
(F-5, A-8) Typical Deposit Analysis %
C – 0.03 Typical Deposit Analysis %
Typical Deposit Analysis %
Mn – 1.21 C – 0.06
C – 0.07 Si – 0.51 Mn – 1.19
Mn – 1.63 Cr – 18.80 Si – 0.46
Si – 0.40 Ni – 13.70 Cr – 20.24
Cr – 18.50 Mo – 3.40 Ni – 10.00
Ni – 12.40 Fe – Bal. Cb – 0.60
Mo – 2.21
Fe – Bal.
Fe – Bal. Typical Properties and Ferrite Number of
Weld Deposit as Welded Typical Properties and Ferrite Number of
Typical Properties and Ferrite Number of Weld Deposit as Welded
Weld Deposit as Welded Tensile Strength . . . . . . . . . . .92,000 psi
Yield Strength . . . . . . . . . . . . .69,000 psi Tensile Strength . . . . . . . . . . .80,000 psi
Tensile Strength . . . . . . . . . . .85,000 psi Elongation in 2" . . . . . . . . . . . . . . .35% Yield Strength . . . . . . . . . . . . .64,000 psi
Yield Strength . . . . . . . . . . . . .68,000 psi DeLong Ferrite Number . . . . . . . . . . . . .4 Elongation in 2" . . . . . . . . . . . . . . .36%
Elongation in 2" . . . . . . . . . . . . . . .45%
DeLong Ferrite Number . . . . . . . . . . . .10
DeLong Ferrite Number . . . . . . . . . . . . .4

13
Stainless Steel
Stick Electrodes

410 AC-DC 2209 AC-DC


AWS E410-16 AWS E2209-16
Air-hardening stainless for welding 12 Cr Specially formulated for welding the 22 Cr-5
material. Requires pre and post-weld heat Nii-3 Mo (Type 2205) duplex stainless steels.
treatments. Approvals and conformances: The deposited duplex weld metal offers
AWS Spec A5.4, ASME SFA5.4 (F-5, A-8) combined high strength with improved
pitting and SSC resistance. Approvals and
Typical Deposit Analysis % conformances: AWS Spec A5.4, ASME SFA5.4
C – 0.09 (F-5, A-8)
Mn – 0.55
Si – 0.29 Typical Deposit Analysis %
Cr – 12.30 C – 0.03
Fe – Bal. Mn – 1.01
Si – 0.38
Typical Properties and Ferrite Number of Cr – 22.90
Weld Deposit as Welded Ni – 10.10
Heat Treated for 1 hr. @ 1375°F Mo – 03.00
Tensile Strength . . . . . . . . . . .80,000 psi N – 0.093
Yield Strength . . . . . . . . . . . . .44,000 psi Fe – Bal.
Elongation in 2" . . . . . . . . . . . . . . .24%
Typical Properties and Ferrite Number of
Weld Deposit as Welded
Tensile Strength . . . . . . . . . . .115,000 psi
Yield Strength . . . . . . . . . . . . .90,000 psi
Elongation in 2" . . . . . . . . . . . . . . .27%
DeLong Ferrite Number (Extended) . . . . .34
Impact Strength ... -50°F . . . . . .23 ft•lbf
(Charpy v Notch)

410NiMo AC-DC
AWS E410NiMo-16
Used extensively for welding ASTM CA6NM
castings as well as 410, 410S and 405 base
metals. Better as-welded toughness than 410.
Approvals and conformances: AWS Spec A5.4,
ASME SFA5.4 (F-5, A-8)

Typical Deposit Analysis %


C – 0.02
Mn – 0.68
Si – 0.35
Cr – 12.48
Ni – 04.30
Mo – 0.55
Fe – Bal.

Typical Properties and Ferrite Number of


Weld Deposit as Welded
Stress Relieved for 1 hr. @ 1125°F
Tensile Strength . . . . . . . . . . .134,000 psi
Yield Strength . . . . . . . . . . . .123,000 psi
Elongation in 2" . . . . . . . . . . . . . . .18%

14
¤

15
Stainless Steel Stick Electrodes
Technical Section

Comparative Index of Stainless Steel Electrodes


AWS Class McKay Techalloy Sandvik Lincoln

E308L-16 308/308L Sterling AP Tech Rod 308L-16 – Red Baron 308L MR

E308L-17 308L-17 Sterling Tech Rod 308L-17 19.9. LR Blue Max 308/308L AC/DC

E308H-16 308/308H Sterling AP Tech Rod 308-16 – Red Baron 308/308H MR

E308H-17 308/308H Sterling Tech Rod 308-17 – –

E309L-16 309/309L Sterling AP Tech Rod 309L-16 – Red Baron 309/309L MR

E3096L-17 309L Sterling Tech Rod 309L-17 24.3. LR Blue Max 309/309L AC/DC

E309-17 309-17 Sterling Tech Rod 309-17 – –

E309Mo-17 309 Mo/309MoL – 23.12.2. LR –

E310-16 310 AC-DC Tech Rod 310-16 – Red Baron 310 MR

E312-16 312 AC-DC Tech Rod 312-16 29.9 R –

E316L-16 316/316L Sterling AP Tech Rod 316L-16 19.12.3. LRV Red Baron 316/316L MR

E316L-17 316L-17 Sterling Tech Rod 316L-17 19.12.3. LR Blue Max 316/316L AC/DC

E316H-16 316/316H Sterling AP Tech Rod 316-16 – –

E316H-17 316/316H-17 Sterling Tech Rod 316-17 – –

E317L-16 317L AC-DC Tech Rod 317-16 19.13.4. LR –

E330-16 330 AC-DC Tech Rod 330-16 – –

E347-16 347 AC-DC Tech Rod 347-16 – –

E410-16 410 AC-DC Tech Rod 410-16 – –

E410NiMo-16 410NiMo AC-DC Tech Rod 410NiMo-16 – –

E2209-16 2209 AC-DC Tech Rod 2209 22.9.3. LR (B) –

16
Stainless Steel Stick Electrodes
Technical Section

TECHNICAL SECTION
Schaeffler Constitution Diagram
Nickel Equivalent = Ni + 30C + 0.5Mn

Calculate the nickel and chromium equivalents from


the weld metal analysis. If nitrogen analysis of the
weld metal is not available, assume 0.06% for
GTAW and covered electrodes or 0.08% for GMAW
weld metals.
If the chemistry is accurate, the diagram predicts
the WRC Ferrite Number within ± 3 in
approximately 90% of the tests for the 308, 309,
316, and 317 families.

Chromium Equivalent = Cr + Mo + 1.5Si + 0.5Cb(Nb)

DeLong Constitution Diagram


Nickel Equivalent = Ni + 30C + 0.5Mn

Comparison with Schaeffler Diagram:


1. The Nickel Equivalent allows for a nitrogen
pick-up of 30N.
2. Ferrite Numbers for 308, 308L, and 347 covered
electrodes are similar. The higher alloy 309,
316, and 317 families have
about 2 to 4 higher FN on this diagram.
3. Generally, this diagram correlates better with
GTAW and GMAW weld metals because it allows
+ for nitrogen pick-up.
4. The Schaeffler austenite-martensite boundary has
been included here for reference.

Chromium Equivalent = Cr + Mo + 1.5Si + 0.5Cb(Nb)

1992 WRC Constitution Diagram


Nickel Equivalent = Ni + 35C + 20N + 0.25Cu

Comparison with Schaeffler and DeLong Diagrams:


1. Considered more accurate for predicting ferrite
in higher-alloyed stainless steels.
2. Copper (Cu) has been added to help determine
the FN of duplex stainless
steel welds.
3. This diagram should be limited to welds that
contain less than 3Mo, less than 1Si, less than
10Mn and less than 0.2N.
4. A = Entirely austenite
AF = Austenite with some ferrite
FA = Ferrite with islands of austenite
F = Ferrite alone

Chromium Equivalent = Cr + Mo + 0.7Cb(Nb)

17
Stainless Steel Stick Electrodes
Technical Section

Stainless Steel Stick Electrode Suggested Operating Ranges


AC-DC/Sterling AP and DC Lime Sterling
Electrode Diameter Flat and Vertical Up Flat and Vertical Up
inches mm Horizontal Welding Welding Horizontal Welding Welding

3/32" 2.4 65–80 45–65 50–80 45–65

1/8" 3.2 90–110 60–80 85–120 55–80

5/32" 4.0 125–150 65–85 130–170 65–85

3/16" 4.8 140–190 NR 160–205 NR


1/4" 6.4 210–300 NR — —

NR = Not Recommended

Stainless Steel Electrodes Per Pound


Diameter: 3/32" (2.4 mm) 1/8" (3.2 mm) 5/32" (4.0 mm) 3/16" (4.8 mm) 1/4" (6.4 mm)
McKay Type Length: 10" 14" 14" 14" 14"

DC Lime (-15) 37 15 10 7 —

AC-DC/Sterling AP 34 13 9 6 3
(-16) Smootharc Plus

Sterling (-17) 34 13 9 6 —

Stainless Steel Stick Electrode Pallet Information


Pallet Weight (lb) Pallet Dimensions Number of Units
Length McKay Type Net Gross (est.) Depth Width Height Per Pallet

3/32"–10" DC Lime 792 892 38" 45" 39" 132 (6 lb Cans)


1/8"–14" 1320 1420 38" 45" 39" 132 (10 lb Cans)
5/32"–14" 1320 1420 38" 45" 39" 132 (10 lb Cans)
3/16"–14" 1320 1420 38" 45" 39" 132 (10 lb Cans)

3/32"–10" AC-DC/Sterling AP 792 892 38" 45" 39" 132 (6 lb Cans)


1/8"–14" Smootharc Plus 1320 1420 38" 45" 39" 132 (10 lb Cans)
5/32"–14" 1320 1420 38" 45" 39" 132 (10 lb Cans)
3/16"–14" 1320 1420 38" 45" 39" 132 (10 lb Cans)
1/4"–14" 1320 1420 38" 45" 39" 132 (10 lb Cans)

3/32"–10" Sterling 792 892 38" 45" 39" 132 (6 lb Cans)


1/8"–14" 1320 1420 38" 45" 39" 132 (10 lb Cans)
5/32"–14" 1320 1420 38" 45" 39" 132 (10 lb Cans)
3/16"–14" 1320 1420 38" 45" 39" 132 (10 lb Cans)

All McKay stainless steel electrodes are


Packaging Options stamped with product name and lot
number for complete traceability.

10 & 14-Inch Electrodes


141/2"
3"

6 & 10 lb Hermetically Sealed Can

Note: The same can is used for the 10" and 14" electrodes.
(A spacer is used for 10" electrodes.)

18
Stainless Steel
Wires

STAINLESS STEEL WIRE


PRODUCT LINE OVERVIEW
For over a half century, McKay® has been the acknowledged leader in stainless steel welding

technology. Exceptionally tight internal specifications and controls in all phases of the manufacturing

operation assure the end user the utmost consistency in chemistry, ferrite, welder appeal, and overall quality.

The McKay reputation for having the highest-quality stainless tubular and solid wires in the market is

a reflection of our dedication to perfection. Industries including food processing, medical equipment, pulp &

paper, petroleum refineries, chemical, nuclear, brewery & distillery, and water systems have all benefited

from using McKay high-quality products.

60 lb Coil 60 lb Coil
(Flux-Cored) (Solid Wire)
(In-Flux 410 NiMoT1 only)

25 or 28 lb Plastic Spool 30 lb Plastic Spool


(Flux-Cored) (Solid Wire)

30 lb Plastic Spool
(Metal-Cored Wire)

10 lb Tube
(Cut Lengths)

19
Stainless Steel Tubular Wires
AWS Section

STAINLESS STEEL TUBULAR WIRE Additional Requirements


AWS SECTION Suffix
L
Additional Requirements
Has a Lower carbon content
H Limited to the upper range on the carbon content
AWS Classification of Stainless Steel Tubular Wires Mo Molybdenum added–pitting resistance, creep
strength, ferrite increased

E308LT1-1 Indicates the shielding gas, if any. (See Shielding Chart)


Ni Nickel added–high temperature strength,
corrosion resistance, + ductility

Indicates the welding position. AWS Class and Applications


Indicates that this is a flux-cored wire. Tubular Class Brief Description
Indicates any changes to the original alloy. A E308 Used for welding many dissimilar 300 series
(See Additional Requirements Chart) stainless steels
Indicates what the weld made by this electrode A E309 Used for welding many dissimilar metals–
will have in it. (See Applications Chart) mild steel to stainless steel
Indicates that this is an electrode. A E316 Mo added to help prevent pitting and
increase creep resistance
Positions Chemical Symbols A E317 Even more Mo than E316
A E347 Cb added to prevent corrosion just outside of
1 Flat, Horizontal, C Carbon Increases strength and hardness–
reduces corrosion resistance. the weld bead
Vertical, Overhead
M E410 For welding martensitic stainless steels and
0 Flat and Horizontal only Mn Manganese Improves crack resistance in fully
austenitic welds. used for surfacing carbon steels
F E430 For welding similar alloys and corrosion-
Flat–Usually groove welds, Si Silicon Increased corrosion and scaling resistance.
resistant surfacing
fillet welds only if welded like P Phosphorus Causes cracking if too high. D E2209 For welding similar duplex stainless steels
a “V”. S Sulfur Aids in machining. Cracking problems like P. E2553 For welding Ferralium 255 and other similar alloys
Horizontal–Fillet welds, Cr Chromium Main corrosion and scaling A –Austenitic M –Martensitic F–Ferritic D –Duplex
welds on walls (travel is from resistance element.
side to side). Ni Nickel Better cold toughness– corrosion resistance.
Vertical–Welds on walls (travel Mo Molybdenum High temperature tensile/creep strength- Shielding Gas and Current
is either up pitting corrosion resistance.
Dash Welding
or down). Ti Titanium High temperature stabilizer–age hardening. Number Shielding Gas Current
Overhead–Weld that needs to N Nitrogen Raises strength–minimize grain growth. -1 CO2 DCEP
be done Cb Columbium High temperature stabilizer– -3 None (Self-Shielded) DCEP
upside down. hardening–strengthening.
-4 75–80% Ar/Remainder CO2 DCEP

AWS (A5.22) Stainless Steel Tubular Wire Chemical Composition of Weld Metal Deposit, %
Carbon Chromium Nickel Molybdenum Manganese Silicon
AWS Class C Cr Ni Mo Mn Si

Open-Arc
E308LT0-3 0.03 Max. 19.5–22.0 9.0–11.0 0.5 Max. 0.5–2.5 1.0
E309LT0-3 0.03 Max. 23.0–25.5 12.0–14.0 0.5 Max. 0.5–2.5 1.0
E316LT0-3 0.03 Max. 18.0–20.5 11.0–14.0 2.0–3.0 0.5–2.5 1.0
E410NiMoT0-3 0.06 Max. 11.0–12.5 4.0–5.0 0.40–0.70 1.0 Max. 1.0
Gas-Shielded
E308T1- 4/-1 0.08 Max. 18.0–21.0 9.0–11.0 0.5 Max. 0.5–2.5 1.0
E308LT1- 4/-1 0.04 Max. 18.0–21.0 9.0–11.0 0.5 Max. 0.5–2.5 1.0
E308LT0- 4/-1
E309LT1- 4/-1 0.04 Max. 22.0–25.0 12.0–14.0 0.5 Max. 0.5–2.5 1.0
E309LT0- 4/-1
E316LT1- 4/-1 0.04 Max. 17.0–20.0 11.0–14.0 2.0–3.0 0.5–2.5 1.0
E316LT0- 4/-1
E317LT1- 4/-1 0.04 Max. 18.0–21.0 12.0–14.0 3.0–4.0 0.5–2.5 1.0
E347T1-4/-1 0.08 Max. 18.0–21.0 9.0–11.0 0.5 Max. 0.5–2.5 1.0 Max.
E410NiMoT1- 4/-1 0.06 Max. 11.0–12.5 4.0–5.0 0.40–0.70 1.0 Max. 1.0
E2209T1- 4/-1* 0.04 Max. 21.0–24.0 7.5–10.0 2.5–4.0 .05–2.0 1.0
E2553T1-4/1
Note: All products listed above also require the following: 0.04 Max. Phosphorus, 0.5 Max. Copper, 0.03 Max. Sulfur *Requires 0.08–0.2 of Nitrogen

20
Stainless Steel
Wires

Stainless Steel Open-Arc Tubular Wires


McKay ® In-Flux® O Wires are designed for joining and cladding in the flat and horizontal positions. These products perform well in field
fabrication or in drafty shop conditions, because they do not require external shielding gas.
McKay Product AWS Class Positions McKay Product AWS Class Positions

In-Flux 308L-O E308LT0-3 Flat, Horizontal In-Flux 316L-O E316LT0-3 Flat, Horizontal

In-Flux 410NiMo-O E410NiMoT0-3 Flat, Horizontal


In-Flux 309L-O E309LT0-3 Flat, Horizontal

Stainless Steel Gas-ShieldedFlux-cored Tubular Wires


McKay ChromaWeld™ LT0 and LT1 Stainless wires are truly a premium stainless gas shielded flux-cored product. ChromaWeld™features a
bright, flat bead profile, clean easy slag release, minimal spatter, higher moisture resistance, and excellent overall weld bead appearance
combined with excellent welder appeal.
McKay Product AWS Class Positions McKay Product AWS Class Positions

ChromaWeld 308LT1 E308LT1-4/-1 All ChromaWeld 316LT1 E316LT1-4/-1 All

ChromaWeld 309LT1 E309LT1-4/-1 All In-Flux 410NiMoT1 E410NiMoT1-4/-1 All

Stainless Steel Gas-Shielded Metal-Cored Tubular Wires


McKay Goldcor wires are designed to meet the needs of chemical/food service/automotive exhaust fabricators that have poor to fair fit up
and desire a metal-cored wire that can produce a soft arc at superior welding speeds.

McKay Product AWS Class Positions

Goldcor 308LSi EC308LSi Flat, Horizontal

Goldcor 309LSi EC309LSi Flat, Horizontal

Goldcor 316LSi EC316LSi Flat, Horizontal

21