Destructive Testing
Destructive Testing
Destructive Testing
4. Quality control
STANDARD TEST METODS
(For Mechanical Testing)
TYPE ASTM BS IS
Tensile E8 EN10002-1 1608,1521
Bend E190 EN287-1 1599
Impact E23 EN 10045-21757
Hardness E10(Brinell) BS 240-1 1500
E18(Rockwell) BS 891-1 1586
E 92(Vickers) BS 427 1501
STANDARDS & CODES FOR DESTRUCTIVE
TESTING
ASTM-A370 : Mechanical Testing of Steels
AWS-B4 : Standard methods for Mechanical testing of welds
BS-709 : Destructive testing for fusion welded Boiler
drums.
IBR Ch.-V : Fusion Welded Boiler Drums.
IBR Ch.-Viii : Qualification test for Welders.
IBR Ch.-XII : Shell type Boiler construction
AWS 5.1,5.4,5.5 : Electrode Qualification Tests
IS 814,5206,1395 : Electrode Qualification Tests
ASME Sec.IX : Procedure & performance Qualification of welding
B1 T2 B2
T1 B2 B1
weld
M
B
m
250 mm
16
406 mm mm
TEST PIPE & TUBE FOR PERFORMANCE
QUALIFICATION (as per IBR
Macro
Root
Face
weld
Root
250mm
Macro Face
Discard Discard
Reduced Sec. Tensile Specimen
Root Bend
Face Bend 300mm
Root Bend
Face Bend
Reduced Sec. Tensile Specimen
Discard Discard
250mm
QW-463.1(a) : Less than 3/4” PLATES
PROCEDURE QUALIFICATION
(ASME SEC. IX)
Discard Discard
Side Bend
Reduced Sec. Tensile Specimen
Side Bend
300
Side Bend
Reduced Sec. Tensile Specimen
Side Bend
Discard Discard
250
QW-463 1(b) :Over 3/4” PLATES
WELDER QUALIFICATION TEST
(API 1104)
Top Pipe
Nick-break
Under
60.3
Top Pipe Root or
Root-bend Side Bend
Nick-break
Grater than 60.3
less than or equal to
114.3mm
Nick-break
Greater than
114.3mm
but less or equal
to 323.8mm
Nick-break
Root or Root or
Side Bend Side Bend
PROCEDURE QUALIFICATION
(API 1104)
Top Pipe
Nick-break
Under
60.3
Top Pipe Root or
Root-bend Side Bend
Nick-break
Greater than 60.3
Nick-break
tensile Face or
Side Bend
PROCEDURE QUALIFICATION
(API 1104)
Top Pipe
Root or Send Bend Face or Side Bend
Tensile
Nick-Break
Root or Send Bend
Tensile
Nick-Break
Face or Side Bend
Greater than
323.8mm
Face or Side Bend
Root or Side Bend
Nick-Break
Nick-Break
Tensile
Tensile
Face or Side Bend Root or Send Bend
WELDER QUALIFICATION
TEST (API 1104)
Top Pipe
Root or Side Bend
Tensile
Nick-Break
Nick-Break
Tensile
Face or Side Bend
Greater than
323.8mm
TRANSEVERSE
TENSILE
ALL WELD
TENSILE
ELECTRODE QUALIFICATION TEST(AS PER AWS)
15 IMPACT SPECIMEN
(5Nos.)
WELD
25
25
DISCARD DISCARD
ALL WELD TENSILE SPECIMEN (as per IS)
R5
10±0.09 12 min
G L 50
PL 60
70mm min
FOR SIZE 4mm AND ABOVE
Ø12.7±0.25 Ø19.1
GL 50.8 ±0.13
SL PL 57.1 SL
Ø6.4±0.13 Ø 9.5
GL 25.4 ±0.13
SL GL 31.8 SL
W
SL PL SL T
RECTANGULAR TENSILE TEST SPECIMEN
(FOR PLATE as per ASTM E8M )
13 min
40 50
200
75 75 5min.
225
ASTM 5d 50 mm
BS 5d 5.65A
IBR 4d 4A
IS 5d 5.65 A
NICK-BREAK TEST SPECIMEN
AS PER API 1104
3.17mm
19mm,
min. 25mm
230mm
NICK-BREAK TEST SPECIMEN
AS PER API 1104
19mm Weld
Wall thickness
1. Guided bend
2. Free Bend
ROOT BEND TEST
t
BEND SAMPLE OF 40 mm THICK PLATE
IN COLD WIRE ADDITION SAW
ROOT BEND TEST
3t
t
1.5t
5.2t
FACE BEND TEST
3t
t
1.5t
5.2t
SIDE BEND TEST
3t
W
t
5.2t
STRICKER
Specimen
Specimen Supporter
10±0.025
2±0.1
10 ±0.025
45°±0.1°
27.5
55±0.1
5±0.1 10±0.025
2 10 ±0.025
27.5
55±0.1
10
2
75 27.5 10
IMPACT TEST SPECIMEN
AS API 5L (SR 5.3)
Max.13.5 mm Min. 28 mm Max.13.5 mm
SPECIMEN
SPECIMEN
SUPPORTER
200x
MICRO STRUCTURE OF BASE METAL
MICRO STRUCTURE OF SAW
WELD METAL
MICRO STRUCTURE OF HAZ IN SAW
MICRO PHOTOGRAPH AT THE CRACK
ORIGIN (200 x)