Technical Data Sheet

Secondary Insulation

Epoxylite® E 230
Two-Component Epoxy Impregnating Resin

ELANTAS PDG, Inc.


5200 North Second Street
St. Louis, MO 63147
USA
Tel +1 314 621-5700
Fax +1 314 436-1030
[email protected]
www.elantas.com
Epoxylite® E 230 Epoxy
Product Description Application Methods

Epoxylite® E 230 Epoxy is a two-component, low Trickle


temperature curing, 100%-solids resin system. Brush on

Areas of Application Transportation / Storage

Impregnation of motor and transformer windings Store below 25°C / 77°F in a dry controlled
including high-speed armatures environment out of direct sunlight. This material
should be suitable for use stored under these
Protective overcoat for motor windings conditions in the original sealed containers for
twelve (12) months from the date of shipment.
Features and Benefits
Failure to store the product as recommended
• Excellent penetration in trickle above may lead to deterioration in product
application performance.

• High bond strength Mix individual components thoroughly before


use.
• Chemical, refrigerant and moisture
resistant Health / Safety

• Fast cure with low heat Refer to the Material Safety Data Sheet.

• Ideal for appliance motors and other


high-speed rotating devices

Typical Properties of Material as Supplied

Property Conditions Value Units


® ®
Epoxylite Epoxylite
E 230 Resin C 230 Hardener

Viscosity 25°C / 77°F 10,000 – 15,000 100 - 500 cP

Weight per Gallon 25°C / 77°F 9.5 – 9.9 8.4 – 8.8 pounds
248 > 94 °C
Flash Point ASTM D93
478 > 201 °F
Parts by weight 100 20
Mix Ratio
Parts by volume 100 22.6

®
Epoxylite E 230 R02 07/28/11 Page 2 of 3
Epoxylite® E 230 Epoxy
Typical Properties of Mixed Materials

Property Conditions Value Units


Viscosity 25°C / 77°F 3,000 - 6,000 cP

Gel Time 25°C / 77°F – 250 grams 15 - 25 minutes

Application / Curing Schedule

Preheat unit to 85 - 95°C / 185 - 203°F

Trickle mixed resin onto unit and allow to gel. Post-cure 15 minutes at 100°C / 212°F. Allow 2 - 7 days
to develop full properties.

Alternatively, allow to gel at room temperature and post-cure for 16 hours at 60°C / 140°F.

Cure schedule is based on time after the unit reaches the specified temperature.

Typical Mechanical Properties

Property Conditions Value Units


Helical Coil Bond Strength 25°C / 77°F 40 pounds
ASTM D2519 over MW 35 150°C / 302°F 4 pounds
Hardness Shore D 75 - 85

R-22 Extractable Material NEMA RE-2 < 1.0 %

Water Absorption 24 hours @ 25°C / 77°F 0.2 %

Typical Electrical Properties

Property Conditions Value Units


Dielectric Strength
25°C / 77°F - 3 mils 1700 volts/mil
ASTM D149
Volume Resistivity ASTM D257 – 25°C / 77°F 1.1 x 1015 ohm-cm

Dielectric Constant 1 kHz – 25°C / 77°F 3.8

Dissipation Factor 1 kHz – 25°C / 77°F 0.03

The above properties are typical values and are not intended for specification use.

ELANTAS PDG, Inc. warrants the chemical composition of its products within stated tolerances, but does not guarantee that a
product will be appropriate for any particular application. Any recommendation, performance of tests or suggestion is offered merely
as a guide and is not a substitute for a thorough evaluation by the user. No representative of ELANTAS PDG, Inc. has the authority
to offer a warranty that a product will perform satisfactorily in manufacturing a product and no such representation should be relied
upon.

®
Epoxylite E 230 R02 07/28/11 Page 3 of 3

You might also like