Sparcast LW 50

SPARCAST LW 50 is a high-strength, low thermal conductivity castable insulating material with a maximum service temperature of 2300°F. It has a dry castable density requirement between 56-65 lbs/cu.ft and approves water content for pouring of 5.0-5.5 gal/100 lbs. Its thermal conductivity remains low at 1.8 BTU/hr/ft2/°F/in from 500°F-1500°F. SPARCAST LW 50 is available in bags and bulk bags that must be stored in dry conditions.
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
0% found this document useful (0 votes)
106 views1 page

Sparcast LW 50

SPARCAST LW 50 is a high-strength, low thermal conductivity castable insulating material with a maximum service temperature of 2300°F. It has a dry castable density requirement between 56-65 lbs/cu.ft and approves water content for pouring of 5.0-5.5 gal/100 lbs. Its thermal conductivity remains low at 1.8 BTU/hr/ft2/°F/in from 500°F-1500°F. SPARCAST LW 50 is available in bags and bulk bags that must be stored in dry conditions.
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
You are on page 1/ 1

INSULATING SPECIALTIES

PRODUCT DATA

SPARCAST LW 50
SPARCAST LW 50 is a 2300°F insulating castable with high strength and low thermal
conductivity.
PHYSICAL PROPERTIES
Maximum Service Temperature 2300°F
Dry Castable Requirement 56 - 65 lbs./cu.ft.
Approximate Water for Pouring 5.0-5.5 gal./100 lbs.
Bulk Density after 220°F 76 - 87 lbs./cu.ft
Modulus of Rupture
After Drying at 220°F 100-200 lbs/sq.in.
After Heating to 1500°F 100-200 lbs/sq.in
After Heating to 2000°F 100-200 lbs/sq.in
Cold Crushing Strength
After Drying at 220°F 300-700 lbs/sq.in.
After Heating to 1500°F 300-700 lbs/sq.in
After Heating to 2000°F 400-800 lbs/sq.in
Linear Change, %
After Drying at 220°F 0.0 to -0.5
After Heating to 1500°F 0.0 to -0.8
After Heating to 2000°F 0.0 to -1.2
Typical Chemical Analysis, %
Al2O3 40.8
SiO2 37.6
CaO 13.7
Fe2O3 3.4
TiO2 1.9
MgO 0.6
Alkalies 2.0
Thermal Conductivity
Temperature °F BTU/hr/ft2 /°F/in.
500 1.8
1000 1.8
1500 1.8
SPARCAST LW 50 is available in 55# bags and various size bulk bags, palletized and
shrink-wrapped.
NOTE: CASTABLE MUST BE STORED IN DRY PLACE
Data shown are average results of standard ASTM tests unless otherwise noted. Results may vary subject to variations in
manufacturing, testing, and installation procedures in the field.

CALDERYS USA
917 Francis St. W, Jacksonville, AL 36265
TEL : (256) 435-9342 - FAX : (256) 435-9373 Date : 08/03/18

You might also like