Specialty Metals – Wire Products

UNS N07750
Inconel® alloy X750 W. Nr 2.4669

Inconel® X750 is a precipitation hardenable Nickel-Chromium alloy with high strength at temperatures up to 1300oF (704oC)
and oxidation resistance up to 1800oF (982oC). Inconel® X750 offers excellent resistance to relaxation and as a result it is
widely used for springs operating at elevated temperatures.
Applications include: springs operating from cryogenic temperatures up to 1300oF (704oC), fasteners and components
requiring resistance to high temperature and corrosive environments.
Industries supplied include: Oil & Gas Extraction and Processing, Nuclear, Aerospace, Power Generation and Automotive
Nominal Composition
Ni Cr Fe Ti Al Cb (Nb) Mn Si C S Cu
min 70.0 14.0 5.0 2.25 0.40 0.70 1.0
max 17.0 9.0 2.75 1.0 1.20 0.50 0.08 0.01 0.5
Physical Properties
At 70oF At 1000oF At 20oC At 538oC
3
Density 0.299 lb/in 8.28 g/cm3
Modulus of Elasticity (E) 31.0 x 106 psi 26.7 x 106 psi 214 GPa 184 GPa
Modulus of Rigidity (G) 12.0 x 106 psi 82.7 GPa
Coefficient of Expansion 7.8 µin/in.-°F (70oF to 1000oF) 14.5 µm/m-°C (20oC to 538oC)
Electrical Resistivity 20.1 µ ohm.in 122 µ.cm
Thermal Conductivity 83 Btu-in/ft2hr-°F 12.0 W/m-K
Applicable Specifications
Wire & Bar AMS 5698, AMS 5699, AMS 5778, NACE MR0175 (ISO 15156-3), ASTM B637, AMS 5667, AMS 5668, AMS 5670
Typical Mechanical Properties – Spring Applications
Condition Heat Treatment Tensile Strength Suggested Operating Conditions
2000 – 2200oF 130 ksi max
Annealed
(1093 – 1204oC) (896 MPa) max
130 – 165 ksi
No.1 Temper As supplied condition.
(896 – 1138 MPa)
Optimum resistance to relaxation at
After spring coiling. 165 – 220 ksi
No.1 Temper + Aged temperatures up to 1000oF (538oC)
Age: 1350oF (732oC) for 16 hours. (1138 – 1517 MPa)
with moderate or low stresses.
160 – 220 ksi
Spring Temper As supplied condition.
(1103 – 1517 MPa)
After spring coiling. 180 – 250 ksi Optimum stress and low relaxation
Spring Temper + Aged
Age: 1200oF (649oC) for 4 hours. (1241 – 1793 MPa) at temperatures up to 700oF (371oC)
After spring coiling.
Solution Heat Treat:
Spring Temper + Optimum resistance to relaxation at
2100oF (1149oC) for 2 hours and air cool. 145 - 190 ksi
Solution + Aged temperatures in the range 1000 –
Age Harden at 1550oF (843oC) for 24 (1000 – 1310 MPa)
(3 Step Heat treatment) 1300oF (538 – 704oC).
hours and air cool. Reheat to 1300oF
(704oC) for 20 hours and air cool.
INCONEL® is a registered trademark of the Special Metals Corporation group of companies.
For further information Contact: Elgiloy Specialty Metals - Wire Products
Email: [email protected] 356 N.Cross Street WWW.ELGILOY.COM
Phone: 1 847 695 1900 Sycamore, IL 60178 USA

August 2015

You might also like