100% found this document useful (1 vote)
175 views3 pages

Technical Data Sheet

Doha Waterproof Factory produces high density polyethylene (HDPE) geomembrane and T lock/V stud sheets. The document provides specifications for the material including physical properties like thickness, width, density, tensile strength, elongation and resistance to chemicals, punctures, and temperature. All properties are tested using standardized methods like ASTM. The sheets are intended to have high durability in waterproofing and environmental applications.

Uploaded by

Abdul Basith
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
100% found this document useful (1 vote)
175 views3 pages

Technical Data Sheet

Doha Waterproof Factory produces high density polyethylene (HDPE) geomembrane and T lock/V stud sheets. The document provides specifications for the material including physical properties like thickness, width, density, tensile strength, elongation and resistance to chemicals, punctures, and temperature. All properties are tested using standardized methods like ASTM. The sheets are intended to have high durability in waterproofing and environmental applications.

Uploaded by

Abdul Basith
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
You are on page 1/ 3

Doha Waterproof Factory

4.Data Data
7. Technical Sheets
Sheet
7.Technical
DataData Data
Sheets Sheet
Technical Sheet

Tel+974-44903836- Mob: +974 50191196- P.O. Box 50311 Doha, State of Qatar
Website: www.dohawaterproof.com // Mail: [email protected]
Doha Waterproof Factory
Data Sheet
High Density Polyethylene Geomembrane sheet

S
Test Unit Specificatio Test Method
N
n
1 Material - HDPE ASTM D1238
Melt Flow Rate for g/10
2 ≤ 3.00 ASTM D1238
2.16 kg @ 190°C min.
3 Density g/cm3 ≥ 0.94 ASTM D1505
4 Sheet Color Black
Carbon Black
5 % 2 to 3 ISO/
Content
DIS 6964/ASTMD1603
(if black) 2.5±0.5
Dimension of Sheet
6 Thickness mm 0.75 1 1.5 2.0 2.5
ASTM D5199
Lowest individual
7 mm 0.65 0.90 1.45 1.90 2.4
thickness
8 Width meter 7.5 m ASTM D4801
9 Length meter As required ASTM D4801
Physical Properties
10 Shore Hardness Shore D ≥ 50 ≥ 50 ≥ 50 ≥ 50 ≥ 50 ASTM D2240
Tensile Strength at
11 N/mm ≥11 ≥ 15 ≥ 23 ≥ 29 ≥ 32
Yield
12 Strength at break N/mm ≥20 ≥ 28 ≥ 42 ≥ 52 ≥ 60 ASTM D6693
Elongation at
13 % ≥700 ≥ 700 ≥ 700 ≥ 700 ≥ 700
Break
Water Absorption
14 % ≤ 0.25 ≤ 0.25 ≤ 0.25 ≤ 0.25 ≤ 0.25 ASTM D570
(24 hrs)
15 Tear resistance N ≥ 93 ≥ 125 ≥ 185 ≥ 240 ≥ 310 ASTM D1004
Puncture
16 N ≥ 240 ≥ 350 ≥ 500 ≥ 580 ≥ 700 ASTM D4833
resistance
Brittleness (low
temperature
- No Cracks No Cracks No Cracks No Cracks No Cracks ASTM D746
17 resistance) @ -
75°C
Chemical Resistance
Test on Environmental Resistance of Liner Sheet for 7 days @ 23 ± 2°C
Hydrochloric acid
-
(10%)
Nitric Acid (10%) -
Sulfuric Acid (30%) -
18 Ammonium
- No Characteristic Observation ASTM D543
Hydroxide (60%)
Ethanol -
Sodium Chloride
-
Solution (20%)
ISO Octane (99.5%) -

Tel+974-44903836- Mob: +974 50191196- P.O. Box 50311 Doha, State of Qatar
Website: www.dohawaterproof.com // Mail: [email protected]
Doha Waterproof Factory
Data Sheet
High Density Polyethylene T lock & V stud Sheet
SN Test Unit Specification Test Method Remark
1 Material - HDPE ASTM D1238
Melt Flow Rate for 2.16 kg @
2 g/10 min. ≤ 1.00 ASTM D1238
190°C
3 Density g/cm3 ≥ 0.94 ASTM D1505
4 Sheet Color Black or other color required by customer
5 Carbon Black Content (if black) % 2.5 ± 0.5 ASTM D1603
Dimension of Sheet
V stud T lock
6 Thickness mm
1.5 to 8 1.5 to 4 As Required
ASTM D4801
7 Width meter Max: 2.0 by Customer
8 Length meter As reqd.
Physical Properties
9 Shore Hardness Shore D ≥ 50 ASTM D2240
10 Tensile Strength at Yield MPa ≥ 15
11 Tensile Strength at Break MPa ≥ 24
ASTM D638
12 Elongation at Yield % ≥ 10
13 Elongation at Break % ≥ 700
14 Water Absorption (24 hrs) % ≤ 0.25 ASTM D570
15 Tear Strength N ≥ 120 ASTM D1004
16 Puncture resistance N ≥ 300 ASTM D4833
Brittleness (low temperature
17 - No crack ASTM D746
resistance) @ -75°C
18 Abrasion resistance (wear index) % 0.007 ASTM D4060
19 Coefficient of Static Friction - ≥ 0.5 ASTM D1894
Chemical Resistance
After Test in Below Solutions for 112 days @ 25 ± 3° C
20 Hardness 1-Sec Shore D ≥ 35 ASTM D2240 This is to be
21 Tensile Strength Mpa ≥ 14.5 ASTM D412 used as pre-
22 Elongation at Break % ≥ 600 ASTM D412 qualification
test and
when
material
23 Weight Change % ± 1.5 ASTM D1239 formulations
are changed

Test on Environmental Resistance of Liner Sheet for 7 days @ 23 ± 2°C


Hydrochloric acid (10%) - This is to be
Nitric Acid (10%) - used as pre-
Sulfuric Acid (30%) - qualification
Ammonium Hydroxide (60%) - No Characteristic test and
24 ASTM D543
Ethanol - Observation when
Sodium Chloride Solution (20%) - material
formulations
ISO Octane (99.5%) - are changed

Tel+974-44903836- Mob: +974 50191196- P.O. Box 50311 Doha, State of Qatar
Website: www.dohawaterproof.com // Mail: [email protected]

You might also like