YOU HERE: Steel numbers -> Number 1.11XX OR Steel and cast iron standards -> / EN 10277-4 / EN 10084
/ EN 10297-1
C15R ( 1.1140 )
Grade : C15R
Number: 1.1140
EN 10277 - 4 : 2008 Bright steel products. Technical delivery conditions. Case hardening steels
EN 10084 : 2008 Case hardening steels. Technical delivery conditions
Standard:
EN 10297 - 1 : 2003 Seamless circular steel tubes for mechanical and general engineering
purposes. Non-alloy and alloy steel tubes
0.12 - 0.18 max 0.4 0.3 - 0.6 max 0.035 0.02 - 0.04
M e c ha nic a l pr ope r t ie s of gr a de C1 5 R ( 1 .1 1 4 0 )
Rp0.2 0.2% proof strength (MPa) (+C) 380 340 280 240 215
P r ope r t ie s of gr a de C1 5 R ( 1 .1 1 4 0 )
http://www.steelnumber.com/en/steel_composition_eu.php?name_id=173 1/2
3/6/2014 C15R / 1.1140 - steel equivalent, mechanical properties, chemical composition
Weldability: It is a soft carbon-steel, easily cold machinable and weldable without any particular precautions.
Equiva le nt gr a de s of gr a de C1 5 R ( 1 .1 1 4 0 )
Warning! Only for reference
Germany France Italy Spain Sweden Inter
DIN,WNr AFNOR UNI UNE SS ISO
Ck15 XC12 C15 C16k-1 1370 C15M2
Cm15
M e c ha nic a l pr ope r t ie s
M e c ha nis c he Eige ns c ha f t e n
Ca r a c t e r is t ique s m e c a nique s
R eH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d�elasticite minimale
R m Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc
He a t t r e a t m e nt c ondit ions
+A Soft annealed
+AC Annealed to achieve spheroidization of the carbides
+AR As rolled
+AT Solution annealed
+C Cold drawn / hard
+CR Cold rolled
+FP Treated to ferrite-pearlite structure and hardness range
+I Isothermal annealing
+LC Cold drawn / soft
+M Thermo mechanical rolling
+N Normalized
+NT Normalized and tempered
+P Precipitation hardened
+PE Peeled
+QA Air quenched and tempered
+QL Liquid quenched and tempered
+QT Quenched and tempered
+S Treated to improve shearability
+SH As rolled and turned
+SR Cold drawn and stress relieved
+T Tempered
Chemical composition of C15R (1.1140). Equivalent grades of C15R (1.1140). Standards of C15R (1.1140).
Properties of C15R (1.1140). Hardness of C15R (1.1140). Strength of C15R (1.1140). Elongation of C15R (1.1140).
© 2011- 2014 All rights reserved. The contents from this site may not be reproduced.
The entire risk as to use of these content is assumed by you the user
http://www.steelnumber.com/en/steel_composition_eu.php?name_id=173 2/2