Wet Mix Macadam consist of laying spreading and compacting of clean, crushed,
well-graded granular materials on a prepared and approved Granular sub-Base. The
material is well mixed with water and rolled to a dense mass. It shall be laid on one
or more layers as per line and level, grade and cross section shown in the drawing or
as directed by the Engineer. The thickness of single compacted Wet Mixed Macadam
(WMM) Base shall not be less than 75 mm. Maximum thickness of single compacted
layer base can be up to 250 mm upon approval of Engineer.
1. Reference
2. Setting Out.
3. Selection of Material.
4. Equipments.
5. Methods of Operation.
6. Quality Control.
7. Work Safety.
8. Environmental Safety.
1.0 Reference
Reference Documents:-
I) Ministry of Road Transport& Highways Specifications
II) Technical Specifications
III) Relevant Drawings.
IV) IS 2720 Codes.
3.1 Aggregate
Coarse aggregate shall be crushed stone or crusher run as per IRC 109 or clause
406.2.1 of MORT&H specification.
The aggregate shall conform to the grading given in table 406.2.1.2 of technical
specification or IRC 109 -2015. Material finer than 425 micron, shall have Plasticity
Index (PI) less than 6. The final gradation approved within these limits shall be well
graded from coarse to fine and shall not vary from low limit on one sieve to high limit
of adjacent sieve or vice versa.
4.0 Equipments
2. Dumper / Tippers.
4. Water Tanker
5. Paver capable of paving more than 9 meter width.
Proper arrangement shall be made for the lateral confinement of wet mix during
laying. This shall be done by laying materials on adjoining shoulder along with that
of WMM layer. The preparation of mix, spreading of mix and compaction are done
sequentially.
The sequence of operation shall be followed as described in clause: 406.3.3 of
MORT&H.
Wet mix Macadam shall be prepared in an approved WMM mixing plant having
provision for controlled addition of water and forced/positive mixing arrangement.
Optimum moisture for mixing shall be determined in accordance with IS: 2720 (Part
8) after replacing the aggregate fraction retained on 22.4 mm sieve with materials of
passing from 22.4 and retained on 4.75 mm. While adding water, evaporation loss
shall also be taken into account. The mixed material should be uniformly wet and no
segregation shall be permitted.
Immediately after mixing, the aggregate shall be spread uniformly and evenly upon
the approved GSB layer. Materials should neither be dumped in heap nor their
hauling over a partly completed stretch. The first layer will be laid by motor grader
and the second layer mix shall be spread by a WMM paver finisher capable of paving
minimum 4.5m to 9.0m width. The layer may be tested by depth block during
construction. No segregation of materials are allowed. The aggregates should be of
uniform gradation with no pockets of fine materials.
5.4 Compaction
After the mix has been laid on site to the required thickness, grade and camber, then
compaction is carried out with suitable roller to the full depth. For a thickness up to
200mm in a single layer, compaction shall be done with vibratory roller of 80 to 100
KN static weights with plain drum or equivalent capacity roller. Rolling is done from
lower edge towards upper edge longitudinally for the portion having unidirectional
cross fall and super elevation.
Each pass of the roller shall uniformly overlap not less than one third of the track
made in the previous pass. During rolling, grade and cross fall shall be checked and
any high spot or depressions, which become apparent, corrected by adding or
removing fresh materials. The speed of roller shall not exceed 5km/h. Rolling shall
be continued till the density of the layer is achieved 98% of the Maximum Dry
Density.
Rolling should not be done when the WMM layer is soft or yielding or when it causes
a wave like motion. If level difference or irregularities develop during rolling which
exceeds 12 mm when tested with 3 metre straight edge, the surface should be
loosened and premixed materials added or removed as required before rolling again.
In no case the unmixed material be permitted to make up the depressions.
After testing the compaction & level of WMM course the road shall be allowed to dry
for 24 hours. Preferably no vehicular traffic should be allowed on the finished WMM
surface till it has dried and covered with wearing course.
Table 400-12 Physical Requirement of coarse aggregate for Wet Mix Macadam for
Sub-base /Base Courses
2.Vehicles tracks shall be kept moist to prevent flying of dust particles with the
vehicle movement.