Typical Properties Test Method (ASTM) Unit Value: Linear Low Density Polyethylene
Typical Properties Test Method (ASTM) Unit Value: Linear Low Density Polyethylene
Typical Properties Test Method (ASTM) Unit Value: Linear Low Density Polyethylene
LL0220AA
Test method
Typical properties Unit Value
(ASTM)
Resin
MFI@190°C,2.16 kg D1238 gr/10min 2 - 2.5
Density D2839 gr/ml 0.917-0.920
Film *
Tensile Strength@Yield ,MD/TD D638 Mpa 10/9
Elongation@Break,MD/TD D638 % 600/810
Tensile Strength@Break,MD/TD D688 Mpa 40/31
Tear Strength,MD/TD D1922 gr/25mic 90/280
Haze D1003 % 13
°
Gloss(45 ) D2457 Rating 50
¾ Values shown are averages & are not to be considered as product specifications.
Vali-e-Asr Ave. cast stretch films such as oriented tapes. It can also be used as a blending
Tehran - IRAN partner in LDPE or LLDPE in both cast and blown film applications.
LL0220AA offers the following advantages when it processed by the cast
extrusion process:
Tel: − Good balance of mechanical properties.
(+98 21)82122700
− Good optical properties.
− Good cling performance.
Fax:
(+98 21)8867 4126-27
LL0220AA also can be used as compounds for low voltage power cable
insulation or fibre optic jacketing.
LL0220AA should be processed in machinery designed for LLDPE.
Web-site: Melt temperature range in the cast process are normally 240°C-280°C and in
www.arpc.ir lean blends for blown film are 165°C-215°C.
LL0220AA should be stored in the dry condition below the 50°C and avoided
from the exposure of direct sunlight.
E-mail:
[email protected]
* LL0220AA is suitable for food contact.
1 Of 1