Physical Properties Metric English: @strain 2.00 % @strain 2.00 %

This document provides physical, mechanical, electrical, thermal, processing, and component element properties for an aluminum alloy in both metric and English units of measurement. Some key properties include a density of 2.72 g/cc, Brinell hardness of 100, tensile strength of 180 MPa, heat of fusion of 389 J/g, thermal conductivity of 134 W/m-K, melting point range of 507-649°C, and primary composition of 75.2-79.6% aluminum and 16-18% silicon.

Uploaded by

Rahul Sanjayan
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as DOCX, PDF, TXT or read online on Scribd
0% found this document useful (0 votes)
44 views

Physical Properties Metric English: @strain 2.00 % @strain 2.00 %

This document provides physical, mechanical, electrical, thermal, processing, and component element properties for an aluminum alloy in both metric and English units of measurement. Some key properties include a density of 2.72 g/cc, Brinell hardness of 100, tensile strength of 180 MPa, heat of fusion of 389 J/g, thermal conductivity of 134 W/m-K, melting point range of 507-649°C, and primary composition of 75.2-79.6% aluminum and 16-18% silicon.

Uploaded by

Rahul Sanjayan
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as DOCX, PDF, TXT or read online on Scribd
You are on page 1/ 1

Physical Properties Metric English


Density  2.72 g/cc 0.0983 lb/in³
 
Mechanical Properties Metric English
Hardness, Brinell  100 100
Hardness, Knoop  126 126
Hardness, Rockwell A  41 41
Hardness, Rockwell B  63 63
Hardness, Vickers  113 113
Tensile Strength, Ultimate  180 MPa 26100 psi
Tensile Strength, Yield  180 MPa 26100 psi
@Strain 2.00 % @Strain 2.00 %
Elongation at Break  <= 1.0 % <= 1.0 %
Tensile Modulus  81.2 GPa 11800 ksi
Compressive Modulus  82.8 GPa 12000 ksi
Machinability  10 % 10 %
Shear Strength  112 MPa 16200 psi
 
Electrical Properties Metric English
Electrical Resistivity  0.00000640 ohm-cm 0.00000640 ohm-cm
 
Thermal Properties Metric English
Heat of Fusion  389 J/g 167 BTU/lb
18.0 µm/m-°C 10.0 µin/in-°F
@Temperature 20.0 - 100 °C @Temperature 68.0 - 212 °F
CTE, linear   
  22.5 µm/m-°C 12.5 µin/in-°F
@Temperature 20.0 - 300 °C @Temperature 68.0 - 572 °F
Specific Heat Capacity  0.963 J/g-°C 0.230 BTU/lb-°F
Thermal Conductivity  134 W/m-K 930 BTU-in/hr-ft²-°F
Melting Point  507 - 649 °C 945 - 1200 °F
Solidus  507 °C 945 °F
Liquidus  649 °C 1200 °F
 
Processing Properties Metric English
Solution Temperature  496 °C 925 °F
Aging Temperature  232 °C 450 °F
 
Component Elements Properties Metric English
Aluminum, Al  75.2 - 79.6 % 75.2 - 79.6 %
Copper, Cu  4.0 - 5.0 % 4.0 - 5.0 %
Iron, Fe  <= 0.50 % <= 0.50 %
Magnesium, Mg  0.45 - 0.65 % 0.45 - 0.65 %
Manganese, Mn  <= 0.10 % <= 0.10 %
Other, each  <= 0.10 % <= 0.10 %
Other, total  <= 0.20 % <= 0.20 %
Silicon, Si  16 - 18 % 16 - 18 %
Titanium, Ti  <= 0.20 % <= 0.20 %
Zinc, Zn  <= 0.10 % <= 0.10 %