0% found this document useful (0 votes)
45 views1 page

Hardness Test Report: Hardness Value 7075 Casted Al 1 2 3 1 2 3 As-Condition 150 / 3HR 350 / 6HR 500 / 6HR

This hardness test report provides hardness values for an aluminum alloy (7075) and cast aluminum. It shows the hardness measured in different conditions: as-cast, after being heated to 150 degrees C for 3 hours, after being heated to 350 degrees C for 6 hours, and after being heated to 500 degrees C for 6 hours. The values were measured in 3 different locations for each material and condition.

Uploaded by

HARIMETLY
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as DOC, PDF, TXT or read online on Scribd
0% found this document useful (0 votes)
45 views1 page

Hardness Test Report: Hardness Value 7075 Casted Al 1 2 3 1 2 3 As-Condition 150 / 3HR 350 / 6HR 500 / 6HR

This hardness test report provides hardness values for an aluminum alloy (7075) and cast aluminum. It shows the hardness measured in different conditions: as-cast, after being heated to 150 degrees C for 3 hours, after being heated to 350 degrees C for 6 hours, and after being heated to 500 degrees C for 6 hours. The values were measured in 3 different locations for each material and condition.

Uploaded by

HARIMETLY
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as DOC, PDF, TXT or read online on Scribd
You are on page 1/ 1

HARDNESS TEST REPORT

HARDNESS 7075 Casted al


VALUE 1 2 3 1 2 3
As-Condition
150 / 3HR
350 / 6HR
500 / 6HR