CSWIP 3.1 Multiple Question
CSWIP 3.1 Multiple Question
1. Deflection of arc by magnetic forces that can make welding difficult to control .is commonly known as….
A arc initiation
B arc misalignment
C arc blow
D arc construction
3. Which of type of electrode is used for ‘stove-pipe’ welding for over land pipelines construction?
A rutile
B cellulosic
C high recovery rutile
D all of the above
4. The three main types of MMA electrodes used for welding C & C-Mn steels are ……..
5.
A basic cellulosic and rutile
B neutral, Cellulosic and rutile
C basic, Cellulosic and neutral
D rutile low hydrogen and basic
5. A WPS may specify a maximum width of individual weld beads (the’ weave’ width) when welding C-Mn
steels. If the width is exceeded it may cause ……..
TWI 2006
Welding inspection: Multi-choice question paper 2
A arc voltage
B welding speed
C Ferro-silicon in the electrode coating
D current
10. Pipe bores of some materials must be purged with argon before and during TIG welding in order to ----
12. Silicon is added to steel, and the covering of MMA electrodes, in order to give -----
A deoxidation
B improve strength
C improve toughness
D more resistance to hydrogen cracking
13. A fusible insert for TIG welding helps to ------
A reduce porosity
B ` gives controlled root penetration
C avoid the need for a back purge
D all of the above
14. According to AWS 2.4 a weld symbol for the other side is placed --------
15. When low hydrogen MMA electrodes are specified for what type of covering will they have……..
A cellulosic
B rutile
C acid
D basic
16. A hydrogen controlled MMA electrodes can always be recognised by the……..
A EN code letter (or AWS code number)
B electrode length
C Trade name
D color of the covering
(2)
17. According to BS EN 22553 which of the following symbols requires weld toes to be smoothly blended on the
other side
TWI 2006
Welding inspection: Multi-choice question paper 2
22. Weld spatter during MMA welding is most likely to be caused by……..
A excessive current
B incorrect baking and storage of electrode
C a bad batch of electrodes
D all of the above
23. A qualified welding procedure specification is used to…..
A give instruction to the welder
B gives information to the welding inspector
C gives confidence that welds will have the specified properties
D all of the above
24. An arc strike (stray flash) on a steel component is regarded by some codes an acceptable because…..
A it will cause copper contamination
B it may cause hard spots
C it may give cracking
D of both B & C
(3)
25. In a transverse tensile test, brittleness would be indicated if …
TWI 2006
Welding inspection: Multi-choice question paper 2
A there is reduction in cross-section at the position of fractures
B the fracture surface is flat and featureless but has a rough surface
C fractured occurred in the weld metal
D the fracture face shows beach marks
27. What does the number 141 refer to on this drawing symbol?(in tail)
28. The polarity used for TIG welding of all materials, except aluminium and magnesium, is……..
A DC negative
B DC positive
C AC
D any polarity can be used
29. A typical temperature range for baking low hydrogen electrodes is …..
A 150 to 200ºC
B 200 to 250 ºC
C 300 to 350 ºC
D 400 to 450 ºC
30. If welding travel speed is doubled, but the current and voltage remain the same, the heat input will…..
A be reduced by 50%
B be increased by a factor of two
C be about the same
D be reduced by approximately25%
(4)