This document provides information on the chemical composition, mechanical properties, heat treatment processes, and standards of a 20MnCr5 steel. Key points include:
- The steel has a carbon content between 0.17-0.22% and chromium content between 1.00-1.30%.
- Heat treatments include normalizing, hardening, tempering, and stress relieving. Tempering is recommended between 150-700°C.
- Mechanical properties tested include hardness between 278-438 HB, yield strength over 930 MPa, and elongation over 7%.
- The steel conforms to European and other international standards for 20MnCr5 or equivalent grades.
This document provides information on the chemical composition, mechanical properties, heat treatment processes, and standards of a 20MnCr5 steel. Key points include:
- The steel has a carbon content between 0.17-0.22% and chromium content between 1.00-1.30%.
- Heat treatments include normalizing, hardening, tempering, and stress relieving. Tempering is recommended between 150-700°C.
- Mechanical properties tested include hardness between 278-438 HB, yield strength over 930 MPa, and elongation over 7%.
- The steel conforms to European and other international standards for 20MnCr5 or equivalent grades.
This document provides information on the chemical composition, mechanical properties, heat treatment processes, and standards of a 20MnCr5 steel. Key points include:
- The steel has a carbon content between 0.17-0.22% and chromium content between 1.00-1.30%.
- Heat treatments include normalizing, hardening, tempering, and stress relieving. Tempering is recommended between 150-700°C.
- Mechanical properties tested include hardness between 278-438 HB, yield strength over 930 MPa, and elongation over 7%.
- The steel conforms to European and other international standards for 20MnCr5 or equivalent grades.
This document provides information on the chemical composition, mechanical properties, heat treatment processes, and standards of a 20MnCr5 steel. Key points include:
- The steel has a carbon content between 0.17-0.22% and chromium content between 1.00-1.30%.
- Heat treatments include normalizing, hardening, tempering, and stress relieving. Tempering is recommended between 150-700°C.
- Mechanical properties tested include hardness between 278-438 HB, yield strength over 930 MPa, and elongation over 7%.
- The steel conforms to European and other international standards for 20MnCr5 or equivalent grades.
Copyright:
Attribution Non-Commercial (BY-NC)
Available Formats
Download as PDF, TXT or read online from Scribd
Download as pdf or txt
You are on page 1of 2
Quality 20MnCr5
According to standards EN 10084: 2008 Lucefin Group
Number 1.7147 Chemical composition C% Si% Mn% P% S% Cr% max max max 0,17-0,22 0,40 1,10-1,40 0,025 0,035 1,00-1,30 Permissible deviations ± 0.02 + 0.03 ± 0.05 + 0.005 + 0.005 ± 0.05 on the product 20MnCrS5 N° 1.7149 S% 0.020-0.040 permissible deviation on the product ± 0.005% By agreement this steel can be supplied with the addition of lead (Pb) 0.15-0.35% Calcium (Ca) treatment may be supplied on request Temperature °C Hot forming Normalizing Core Carbonitriding Carburizing Hardening Tempering hardening carburizing surf. 1150-850 860-880 860-890 750-930 880-930 810-840 150 air oil-polymer gas oil-polymer 200 (HB 140-201) salt bath salt bath Soft Isothermal Spheroidizing End quench Preheating Stress relieving anealing +A annealing Hardenability welding after welding 750-770 slowly 860 furnace 720-740 furnace 870 welding must be made on the annealing and before 15 °C/h cooling to cooling to 670 water the carburizing until 680 pause 650 after, air pause 150-350 600 furnace cooling after slowly to 400 cooling to 300 AC1 AC3 MS * core pause, after air after air ** carburizing surface (HB max 217) (HB 170-217) (HB 152-201) 730 830 390* 200** Transformation annealing +FP As-rolled Stress relieving 950-1000 quick cooling to 620-650 holding abaut 3 h, after air --- 600-620 (HB 152-201) (HB max 230) Mechanical and physical properties Hot rolled properties obtained from test blanks after core hardening + stress relieving UNI 7846: 1978 Only reference. size Testing at room temperature (longitudinal) mm R Rp 0.2 A% C% Kcu HB test blanks N/mm2 N/mm2 min. min. min. J min. 11 1230-1570 930 7 -- 17.5 363-438 30 930-1230 690 8 -- 20 278-363 for information 63 780-1080 540 9 -- 25 232-327 for information Table of tempering values at room temperature for round Ø 10 mm after quenching at 870 °C in oil HB 426 426 421 421 415 409 395 381 362 336 294 261 240 224 HRC 45.5 45.5 45 45 44.5 44 42.5 41 39 36 31 26.5 22.5 -- R N/mm2 1500 1500 1490 1480 1460 1430 1370 1300 1210 1100 980 875 795 740 Rp 0.2 N/mm2 1060 1140 1190 1230 1240 1240 1220 1180 1090 960 850 750 670 600 A % 11.5 11.9 12.0 12.0 11.9 11.8 11.9 12.2 12.8 14.0 16.0 18.8 21.8 23.2 C % 48 49 50 52 53 55 56 58 60 62 64 67 70 72 Kv J 38 40 40 40 38 38 32 34 75 75 100 128 145 155 HRC carburizing 64.5 64 63 60.5 59 57 -- -- -- -- -- -- -- -- surface Tempering at °C 50 100 150 200 250 300 350 400 450 500 550 600 650 700 20MnCrS5 1.7149 EN 10277-4: 2008 Lucefin Group size Soft annealing +A +SH Soft annealing +A +C Heat treatment +FP +SH Heat treatment +FP +C mm Peeled Reeled Cold drawn for pearlite / ferrite for pearlite / ferrite Ground +SL Peeled Reeled, Ground Cold drawn over to HB max HB max HB HB 5 a) 10 -- 270 -- -- 10 16 -- 260 -- -- 16 40 217 255 152-201 152-250 40 63 217 250 152-201 152-245 63 100 217 250 152-201 152-245 a) for thickness below 5 mm mechanical properties can be agreed before order placement
Forged UNI 8550: 1984 Only reference.
size Testing at room temperature (longitudinal) mm R Rp 0.2 A% L A% T A% Q Kcu L Kcu T Kv L HB over to N/mm2 N/mm2 min min min min J min J min J min for inform. 11 1225-1570 930 7 -- -- 17.5 -- -- 361-438 11 25 930-1225 685 8 -- -- 20 -- -- 278-361 25 50 785-1080 540 9 -- -- 25 -- -- 234-327 mechanical properties obtained from test blanks after core hardening + stress relieving L = longitudinal T = tangential Q = radial EN 10084: 2008 Jominy test HRC grain size 5 min. distance in mm from quenched end 1.5 3 5 7 9 11 13 15 20 25 30 35 40 45 50 -- H min 41 39 36 33 30 28 26 25 23 21 -- -- -- -- -- -- normal max 49 49 48 46 43 42 41 39 37 35 34 33 32 -- -- -- Temperature Mod. of elasticity N/mm2 Rp 0.2 N/mm2 Thermal expansion Testing at °C E long. G tang. Ǿ < 250 mm Ǿ 250-500 [(m/m●K) ●10-6 °C-1 ] 20 210000 80000 -- -- -- 100 205000 78000 -- -- 11.1 200 195000 75000 -- -- 12.1 300 -- -- -- -- 12.9 400 175000 67000 -- -- 13.5 500 -- -- -- -- 14.1 600 155000 59000 -- -- -- Specific heat capacity Density Thermal conductivity Specific electric resist. Conductivity J/(Kg●K) Kg/dm3 W/(m●K) Ohm●mm2/m Siemens●m/mm2 460 7.85 41 0.16 6.25 EUROPE EN ITALY UNI CHINA GERMANY DIN FRANCE AFNOR U.K. B.S. RUSSIA USA AISI/SAE 20MnCr5 20MnCr5 20CrMn 20MnCr5 20MC5 -- 20HG 5120